Continuous or simultaneous chlorine leach and ion exchange resin absorption. The ground carbonaceous ore is mixed with water in the slurry preparation chamber after which it is then transported into the the chlorine leach/resin absorption vessel where the chlorine compound is added after which the ion exchange resin is also added simultaneously to separate gold from the slurry mixture.