Beam, collam and block wall joint should be wiremess fix, if have concrete beam and collam should be chipping and should be rashcoat(tartasha) on wall before plastering. For good plaster and plaster finishing should be plaster thickness 1.5cm.minimum and 2cm. Maximum. Very important make the plaster point on the wall in the lavel and right angle before plastering.